Segondè alumina refractory Castable
Enfòmasyon sou pwodwi
Non pwodwi | Refractory Castable |
Kategori | Ba Siman Castable / High Strength Castable /Segondè Alumina Castable / Lejè Castable |
Konpozisyon | Refractory total, poud ak atach |
Karakteristik | 1.Easy konstriksyon, 2.Bon rezistans salop, 3.Bon rezistans korozyon, 4.Bon rezistans dife, 5.Energy ekonomize ak pwoteksyon anviwònman an. |
Aplikasyon | Lajman itilize nan divès kalite gwo tanperati endistriyèl founo. |
Pwodwi yo | Low Siman Castable | Segondè fòs Castable |
Deskripsyon | Castables ki ba siman refere a nouvo castables ki gen anpil ti lyan siman.Kontni an siman nan castables refractory se jeneralman 15% a 20%, ak kontni an siman nan castables ki ba siman se apeprè 5%, ak kèk yo menm redwi a 1% a 2%. | Segondè fòs mete ki reziste castable konpoze de total fòs segondè, melanj mineral, total fòs segondè ak anti krak ak ajan mete ki reziste. |
Karakteristik | Rezistans chòk tèmik, rezistans salop, ak rezistans ewozyon yo siyifikativman amelyore, depase brik refractory menm jan an. | Segondè fòs, segondè rezistans mete, rezistans enpak, rezistans ewozyon, pèmeyabilite anti-lwil oliv, kontwòl fòm abitrè, entegrite fò, konstriksyon senp, bon pèfòmans konstriksyon, ak sèvis long. |
Aplikasyon | 1.Lining nan divès kalite fou tretman chalè, founo chofaj, founo arbr, fou rotary, kouvèti fou elektrik, tapholes eksplozyon; 2.Self-flowing ba-siman castables yo apwopriye pou pawa segondè-tanperati espre zam pou metaliji espre ak petrochimik katalitik fann reyaktè Mete ki reziste pawa, pawa ekstèn nan tiyo chofaj gwo founo dlo-refwadi, elatriye. | Kouch pawa ki reziste nan salop,depresyon minrè, bec chabon, Hopper ak silo nan metaliji, chabon, pouvwa tèmik, pwodui chimik,siman ak lòt endistri yo, ak gwo founo dife silo melanje, silo SINTERING, feeder, pelletizer, elatriye. |
Pwodwi yo | High Alumina Castable | Lejè Castable |
Deskripsyon | High-alumina castables yo refractorycastables te fè nan matyè premyè segondè-aluminakòm total ak poud, epi ajouteak atachman. | Castable ki lejè a ak dansite esansyèl ki ba se te fè nan siman aluminate, segondè alumina materyèl amann, seramsite, ak aditif. |
Karakteristik | Gen gwo fòs mekanik ak bon rezistans chòk tèmik, rezistans fwotman ak lòt pwopriyete. | Ba dansite esansyèl, ti konduktiviti tèmik, bon efè izolasyon tèmik, segondè fòs konpresiv, asid ak asid rezistans korozyon gaz, izolasyon chalè, izolasyon tèmik, ak absòpsyon dlo ki ba. |
Aplikasyon | Li se sitou itilize kòm pawa enteryè nan chodyèr, gwo founo dife cho eksplozyon recho, founo chofaj, fou seramik ak lòt fou. | Castable ki lejè a ka itilize pou kouch izolasyon tèmik nan gwo-tanperati gwo founo dife endistriyèl ak ekipman yo itilize tou pou pawa nan divès kalite tiyo gaz wo-tanperati. |
Endèks pwodwi
Sou entènèt jwèt Cho eksplozyon recho
Tinèl au
Rotary Kiln
Endistri fè ak asye: sitou itilize pou antretyen ak plak nan founo elektrik arc, founo asye, louch ak lòt ekipman.
Endistri metal ki pa FERROUS: itilize pou plak ak reparasyon nan kwiv, aliminyòm, zenk, nikèl ak lòt founo metal ki pa FERROUS ak konvètisè.
Endistri vè: yo itilize pou antretyen ak travay patch nan founo vè, founo recuit ak lòt ekipman.
Non pwodwi | Low Siman Castable | |||||
ENDEX | RBTZJ-42 | RBTZJ-60 | RBTZJ-65 | RBTZJS-65 | RBTZJ-70 | |
Tanperati Limit travay | 1300 | 1350 | 1400 | 1400 | 1450 | |
Dansite esansyèl (g/cm3)110℃×24h ≥ | 2.15 | 2.3 | 2.4 | 2.4 | 2.45 | |
Fòs koube frèt110℃ × 24h (MPa) ≥ | 4 | 5 | 6 | 6 | 7 | |
Fwad kraze fòs(MPa) ≥ | 110℃ × 24h | 25 | 30 | 35 | 35 | 40 |
CT℃ × 3h | 50 1300℃ × 3h | 55 1350 ℃ × 3h | 60 1400 ℃ × 3h | 40 1400 ℃ × 3h | 70 1400 ℃ × 3h | |
Chanjman lineyè pèmanan@CT℃×3h (%) | -0.5 ~ + 0.5 1300℃ | -0.5 ~ + 0.5 1350℃ | 0~+0.8 1400℃ | 0~+0.8 1400℃ | 0~+1.0 1400℃ | |
Rezistans chòk tèmik (1000℃ dlo) ≥ | ― | ― | ― | 20 | ― | |
Al2O3(%) ≥ | 42 | 60 | 65 | 65 | 70 | |
CaO(%) ≤ | 2-3 | 2-3 | 2-3 | 2-3 | 2-3 | |
Fe2O3(%) ≤ | 2.0 | 1.5 | 1.5 | 1.5 | 1.5 |
Non pwodwi | Segondè fòs Castable | |||||
ENDEX | HS-50 | HS-60 | HS-70 | HS-80 | HS-90 | |
Tanperati limit travay (℃) | 1400 | 1500 | 1600 | 1700 | 1800 | |
110℃ dansite esansyèl (g/cm3) ≥ | 2.15 | 2.30 | 2.40 | 2.50 | 2.90 | |
Modil rupture (MPa) ≥ | 110℃ × 24h | 6 | 8 | 8 | 8.5 | 10 |
1100 ℃ × 3h | 8 | 8.5 | 8.5 | 9 | 9.5 | |
1400 ℃ × 3h | 8.5 1300℃×3h | 9 | 9.5 | 10 | 15 | |
Fwad kraze fòs(MPa) ≥ | 110℃ × 24h | 35 | 40 | 40 | 45 | 60 |
1100 ℃ × 3h | 40 | 50 | 45 | 50 | 70 | |
1400 ℃ × 3h | 45 1300℃×3h | 55 | 50 | 55 | 100 | |
Chanjman lineyè pèmanan (%) | 1100 ℃ × 3h | -0.2 | -0.2 | -0.25 | -0.15 | -0.1 |
1400 ℃ × 3h | -0.45 1300 ℃ × 3h | -0.4 | -0.3 | -0.3 | -0.1 | |
Al2O3(%) ≥ | 48 | 48 | 55 | 65 | 75 | 90 |
CaO(%) ≤ | 4.0 | 4.0 | 4.0 | 4.0 | 4.0 | 4.0 |
Fe2O3(%) ≤ | 3.5 | 3.5 | 3.0 | 2.5 | 2.0 | 2.0 |
Non pwodwi | High Alumina Castable | ||||||
ENDEX | Al2O3(%)≥ | CaO(%)≥ | Refractoriness (℃) | CT℃ × 3h PLC ≤1% | 110 ℃ Apre siye (MPa) | ||
CCS | MOR | ||||||
Clay Bonded | NL-45 | 45 | ― | 1700 | 1350 | 8 | 1 |
NL-60 | 60 | ― | 1720 | 1400 | 9 | 1.5 | |
NL-70 | 70 | ― | 1760 | 1450 | 10 | 2 | |
Siman Bonded | GL-42 | 42 | ― | 1640 | 1350 | 25 | 3.5 |
GL-50 | 50 | ― | 1660 | 1400 | 30 | 4 | |
GL-60 | 60 | ― | 1700 | 1400 | 30 | 4 | |
GL-70 | 70 | ― | 1720 | 1450 | 35 | 5 | |
GL-85 | 85 | ― | 1780 | 1500 | 35 | 5 | |
Low Siman Bonded | DL-60 | 60 | 2.5 | 1740 | 1500 | 30 | 5 |
DL-80 | 80 | 2.5 | 1780 | 1500 | 40 | 6 | |
Fosfat kole | LL-45 | 45 | ― | 1700 | 1350 | 20 | 3.5 |
LL-60 | 60 | ― | 1740 | 1450 | 25 | 4 | |
LL-75 | 75 | ― | 1780 | 1500 | 30 | 5 | |
Silikat sodyòm kole | BL-40 | 40 | ― | ― | 1000 | 20 | ― |
Non pwodwi | Lejè Castable | ||||||
Tanperati limit travay | 1100 | 1200 | 1400 | 1500 | 1600 | ||
110℃ dansite esansyèl (g/cm3) ≥ | 1.15 | 1.25 | 1.35 | 1.40 | 1.50 | ||
Modil rupture (MPa) ≥ | 110℃ × 24h | 2.5 | 3 | 3.3 | 3.5 | 3.0 | |
1100 ℃ × 3h | 2 | 2 | 2.5 | 3.5 | 3.0 | ||
1400 ℃ × 3h | ― | ― | 3 | 10.8 | 8.1 | ||
Fòs kraze frèt (MPa) ≥ | 110℃ × 24h | 8 | 8 | 11 | 12 | 10 | |
1100 ℃ × 3h | 4 | 4 | 5 | 11 | 10 | ||
1400 ℃ × 3h | ― | ― | 15 | 22 | 14 | ||
Chanjman lineyè pèmanan (%) | 1100 ℃ × 3h | -0.65 1000 ℃ × 3h | -0.8 | -0.25 | -0.15 | -0.1 | |
1400 ℃ × 3h | ― | ― | -0.8 | -0.55 | -0.45 | ||
Kondiktivite tèmik (W/mk) | 350℃ | 0.18 | 0.20 | 0.30 | 0.48 | 0.52 | |
700℃ | 0.25 | 0.25 | 0.45 | 0.61 | 0.64 | ||
Al2O3(%) ≥ | 33 | 35 | 45 | 55 | 65 | ||
Fe2O3(%) ≤ | 3.5 | 3.0 | 2.5 | 2.0 | 2.0 |